• Clean the Surface of application well and wet it before application.
  • Mix 9-10 liter of water in the 40 kg of bag depending on thickness of joints to be build up and ensure that no dry powder remains after addition of water.
  • Apply rhino block bonder on dry block surface using trowel to make an even thickness of 3-5 mm.
  • Continue to Place the next Block and repeat the same procedure and remove the excess material.